Hello , Sign In
TLC polyester sheets with aluminum oxide (neutral). We recommend to activate aluminum oxide layers before use by heating 10 minutes at 120 °C.
| Sub Brand | POLYGRAM |
|---|---|
| Material | Polyester Sheets Coated with Aluminum Oxide |
| Surface Chemistry | Aluminum Oxide;Neutral |
| Support Material | Polyester |
| UV Indicator (Yes/No) | Yes |
| pH Stability | 2.0 to 8.0 |
| Binder (Yes/No) | Yes |
| Layer Thickness | 0.2 mm |
| Layer Hardness | Standard;Soft |
| Includes | (25) TLC Polyester Sheets/Foils |
| Temperature Stability | <185 °C |
| Applications | Aliphatic and Aromatic Compounds;Alkaloids;Steroids;Terpenes |
| Storage Temperature | Room Temperature |
| Hazardous Material (Yes/No) | No |